Sign In | Join Free | My disqueenfrance.com
China DONGGUAN LONROY EQUIPMENT CO LTD logo
DONGGUAN LONROY EQUIPMENT CO LTD
DONGGUAN LONROY EQUIPMENT CO LTD
Verified Supplier

2 Years

Home > Differential Scanning Calorimeter >

Automatic Differential Scanning Calorimeter High Resolution DSC Lab Calorimeter Differential Scanning Calorimeter

DONGGUAN LONROY EQUIPMENT CO LTD
Trust Seal
Verified Supplier
Credit Check
Supplier Assessment
Contact Now

Automatic Differential Scanning Calorimeter High Resolution DSC Lab Calorimeter Differential Scanning Calorimeter

Brand Name : LONROY

Place of Origin : Guangdong, China

MOQ : 1

Voltage : 220 V

Protection Class : Ip56

Display Mode : 24-bit color, 7-inch LCD touch screen display

Sensitivity : 0.001 milliwatt

Temperature Resolution : 0.01 degree Celsius

Power Range : 0 to ±500 milliwatts

Temperature Range : Room temperature to 1450℃ (air-cooled)

Rate of Temperature Increase : 1~80℃/min

Temperature Fluctuations : ±0.1℃

Temperature Repeatability : ±0.1℃

Noise : 0.001 milliwatts

Power Resolution : 0.001 milliwatt

Power Precision : 0.01 milliwatts

Temperature Control Method : Heating, constant temperature, cooling, circulation (fully automatically controlled)

Data Interface : Standard USB interface

Contact Now

Automatic Differential Scanning Calorimeter High Resolution DSC Lab Calorimeter Differential Scanning Calorimeter

Automatic Differential Scanning Calorimeter High Resolution DSC Lab Calorimeter Factory Price

Product Description

Technical Features

1. Dual temperature probes ensure high repeatability in sample temperature measurement.

2. The digital gas mass flowmeter can automatically switch between two gas flow paths, with a fast switching speed and a short stabilization time.

3. Standard samples are provided as standard equipment, facilitating customers' calibration of the temperature coefficient.

4. The instrument is equipped with a fully automatic calibration function.

5. The installation process has been improved. All parts are fixed mechanically, completely eliminating the contamination of the internal gel in the furnace body to the differential thermal signals.

6. The software is adaptable to various resolution computer screens. The software automatically adjusts the display mode of each curve according to the size of the computer screen. It supports laptops, desktop computers, and is compatible with operating systems such as WIN2000, XP, WIN7, WIN8, and WIN10.

7. Supports user-defined programming of programs, enabling complete automation of measurement steps. The software offers dozens of instructions, allowing users to flexibly combine various instructions according to their own measurement procedures and save them. Complex operations are simplified to a single-click operation.

8. Industrial-grade wide-screen touch structure, providing rich display information, including set temperature, sample temperature, oxygen flow rate, nitrogen flow rate, differential thermal signal, various switch states, and flow reset.


Automatic Differential Scanning Calorimeter High Resolution DSC Lab Calorimeter Factory Price

Technical Specification

Range

0 to ±500 milliwatts

Temperature Range

Room temperature to 1450℃ (air-cooled)

Rate of Temperature Increase

1~80℃/min

Temperature Resolution

0.01 degree Celsius

Temperature Fluctuations

±0.1℃

Temperature Repeatability

±0.1℃

Noise

0.001 milliwatts

(Power) Resolution

0.001 milliwatt

(Power) Precision

0.01 milliwatts

Sensitivity

0.001 milliwatt

Temperature Control Method

Heating, constant temperature, cooling, circulation (fully automatically controlled)

Curve Scanning

Temperature rise scan

Atmosphere Control

Instrument automatic switching

Display Mode

24-bit color, 7-inch LCD touch screen display

Data Interface

Standard USB interface

Parameter Standards

Equipped with standard substances (tin); users can independently calibrate temperature and enthalpy

Automatic Differential Scanning Calorimeter High Resolution DSC Lab Calorimeter Differential Scanning CalorimeterAutomatic Differential Scanning Calorimeter High Resolution DSC Lab Calorimeter Differential Scanning CalorimeterAutomatic Differential Scanning Calorimeter High Resolution DSC Lab Calorimeter Differential Scanning CalorimeterAutomatic Differential Scanning Calorimeter High Resolution DSC Lab Calorimeter Differential Scanning Calorimeter


Product Tags:

high resolution DSC lab calorimeter

      

automatic differential scanning calorimeter

      

DSC calorimeter with warranty

      
China Automatic Differential Scanning Calorimeter High Resolution DSC Lab Calorimeter Differential Scanning Calorimeter wholesale

Automatic Differential Scanning Calorimeter High Resolution DSC Lab Calorimeter Differential Scanning Calorimeter Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: DONGGUAN LONROY EQUIPMENT CO LTD
*Subject:
*Message:
Characters Remaining: (0/3000)
 
Inquiry Cart 0